Determination of reactivity
Description
B-time determination on the B-Timing Plate provides information on the curing behavior of resins capable of heat-hardening, namely the reaction time at a given temperature after which resins (solid, liquid, or solvent-containing resins of a known concentration) change to the B-state. Our standard B-Timing Plate has four depressions in the heating plate, accepting one sample each. Plates without depressions are also available.
The temperature is precisely controlled with our temperature controller TCT-1 with integrated Stopwatch.
Technical Data
B-Timing Plate
| Voltage | 115 VAC or 230 VAC, 50/60 Hz |
| Power | 160 W |
Temperature-Controller TCT-1 with Stopwatch
| Voltage | 100 …240 VAC, 50 / 60 Hz |
| Power | 200 VA with connected B-Timing plate |
| Connections | 8 Pol Binder plug, power line and sensor |
| Sensor | Pt100, EN60751 |
| Temperature range | 30°C … 200 °C (on request 250 °C) |
| Accuracy | +/- 0,5°C |
| Additional sensor | 1 x Thermo connector type K, EN 60584, for the surface temperature |
| Main switch | on the back side |
| Fuses | 2 pcs F3,15A L250 VAC |
Standards
DIN 16 916 or DIN EN ISO 8987